Your shopping cart is empty.

Reducing the risk of Galvanic Corrosion


PLEASE READ THIS IN CONJUNCTION WITH THE ELECTROLYIC COMPATABILITY TABLE.

When two dissimilar metals or two similar metals which differ only slightly in chemical composition are in contact in the presence of moisture (e.g. a damp or humid atmosphere) electrolytic or galvanic corrosion can occur.

This is caused by the generation of a minute current that causes one of the metals to be eaten away.

Metals furthest apart in an electrolytic series will corrode most rapidly. The Electrolytic compatability table shows the possible extent of electrolytic corrosion for comparison purposes, as well as the differences in corrosion rates for different metal combinations.

A straight line is drawn between the two metals being considered; one metal selected from the left hand list and the other from the right hand list. The centre column number scale represents the degree of possible corrosion activity.

A large number indicated high possibility of electrolytic activity, whilst a low number indicated a better combination for resisting electrolytic corrosion. The left and right hand material columns also indicate which metal will be protected and which will be attacked by corrosion.

Example:

  • Example A: connecting inconel (passive) on the left scale, with Magnesium Alloys on the right scale, gives a value of 27. This is a high electrolytic risk situation, with the inconel being protected at the expense of the Magnesium Alloy.
  • Example B: connecting inconel (passive) with Copper/Nickel alloys gives a value of 3. This is obviously a better corrosion resisting combination.

A greater corrosion rate than indicated can result if a small Anode is in contact with a large Cathode since the electrical current density is increased at the Anode.

Where it is not possible to use materials that will resist corrosion then use a protective agent such as Tef Gel or use rubber/nylon washers If the materials are likely to be exposed to particularly corrosive conditions.


Prevention

To avoid galvanic corrosion, the dissimilar metals need to be isolated from each other and not in contact. Nylon or EPDM washers can be used as well as Tef-Gel.


The contact between dissimilar metals in the presence of an electrolyte, like salty water, can create galvanic corroson. The chart shows to what extent this can occur.

By using such products as nylon/epdm washers or tef gel this can be prevented or diminished.


Electrolytic Compatability Chart - Anzor

Other useful information

NB: This information is provided as a guide only and Anzor does not accept liability for the application of this information.

For advice about stainless steel, contact the Nickel Institute

Learn Something New

To receive useful info and product updates add your details below

Recently Viewed
Anzor Wallchart

Wall Chart

Request a hardcopy of our product wall chart or download a PDF.

Anzor Catalogues

Standard Catalogues

Download a PDF of our paper based catalogue.

You are subscribed to push notifications but they are not enabled in your browser.
Please either enable push notifications here or unsubscribe here.